How To Solve The Problems In The Process Of Solventless Composite

Here, we give a detailed analysis of the undesirable phenomenon in the solventless composite and solventless laminating machine, such as the uniform winding, poor coating effect, etc and how to solve the problems.

Poor Coating Performance

1. The pressure of the transfer roller is not enough.

2. Mechanical brake adjustment error of transfer roller.

3. The coating roller is not clean well.

4. The poor finish of the glue pressure roller, the transfer roller, or the composite roller.

Poor Coating Performance Of Thin Film Edge

1. The adhesive close to the baffle does not replace for a long time, as long as it often swings the spray nozzle to maintain the adhesive fresh.

2. The coated pressure roller of the composite roller has glue or other impurities.

Uneven Section Of Rewinding

1. The glue amount is too large.

2. The cooling performance of the back film roll which is from the composite roller, is poor.

3. Tension is not suitable.

4. The flatness of the squeeze roll in the rewinding is poor.

5. The glue coating amount in the left and right sides of the film is too large and it is best to control the difference within 0.2g.

6. The paper core is not aligned with the film.

 

White Spot

1. Low glue coating

There is not enough adhesive to penetrate into ink. At this time, it appears as a small and uniform spot in the entire composite film. The solutions are to appropriately increase the amount of glue and adjust the composite temperature and composite pressure.

2. The glue portion, the composite portion of the rollers have a poor surface finish. At this time, it is expressed as partial intermittent repeated spots. It can be judged by measuring the spacing of the two spots to find that which rolls have foreign matter and clean up.

3.The tension of substrate film is uneven and wrinkles before entering the composite roller, resulting in poor partial composite performance, and the bubbles will appear, the macroscopic manifestation is a white spot. The solution is to adjust the deflection roller and keep the film neat before entering the composite roller. The tension can be appropriately adjusted or replace film.

4.The pressure of the composite portion of the glue portion is not properly set.

5. The solubility of the ink and adhesive is not good, white spots will occur at no adhesive penetrated ink, and the suitable adhesive or ink should be replaced.

For more information, please visit the article page of the undesirable phenomenon in solventless composite.

 оценок 0

Автор: Статус: offline pinkledstone
просмотров: 11
Поделиться в:   icon   icon   icon   icon   icon    


Чтобы добавить комментарий Вы должны зарегистрироваться или войти если уже зарегистрированы.

(Вы можете отправить комментарий нажатием комбинации клавиш Ctrl+Enter)